GX binder grades cover different bonding-temperature duties; LS mortar grades serve masonry joints. KTS-2 is a jointing option for carburizing and nitriding heat-treatment furnaces.
Typical applications
- Refractory-to-refractory bonding and furnace masonry
- Selected refractory-fiber and fiber-to-metal bonding interfaces

Technical specifications
| Property / grade | High-temperature binders | High-temperature mortars | Carburization-resistant mortar | |||
|---|---|---|---|---|---|---|
| GX-2 | GX-3 | LS-2 | LS-3 | KTS-2 | ||
| Service temperature (°C) | 1200 | 1500 | 1300 | 1550 | 1350 | |
| Consumption (kg per unit area; denominator unreadable) | 1.8-3.6 | 2-3.5 | 4-5 | 4-5.5 | 3.5-4.5 | |
| Bond strength (MPa) | 105℃ | 4.5 | 4.0 | 5.6 | 7.0 | 6 |
| 1100℃ | 8.9 | 8.1 | 8.2 | 9.1 | 8.5 | |
| 1300℃ | 9.1 | 10.2 | 10.3 | 11.2 | 10.8 | |
| 1400℃ | — | 11.5 | — | 13.1 | 12.5 | |
| Consistency (mm) | 210 | 195 | 180 | 160 | 170 | |
| Strength (MPa; test name unclear in reference) | 14 | 11 | 9 | 8 | 8 | |
| Permanent change after drying (%) | -1.2 | -1 | -0.7 | -0.7 | -0.9 | |
Data clarification
Published reference figures are not a certified specification for the quoted batch. Confirm the grade, test method, furnace conditions and acceptance requirements before ordering. A dash means no value was stated; classification temperature is not a continuous-service guarantee.
- The narrative gives LS-3 a 1500°C duty, while its table states 1550°C. Confirm the supplied grade before use.
- The consumption unit denominator is unreadable, and the test labelled strength in the reference is ambiguous. Numerical entries are retained but are not verified test specifications.
Information for quotation
Send the product or grade, furnace zone, operating temperature and atmosphere, dimensions or lining drawing, quantity and delivery destination.