Extruded Batts
Internal channels reduce furniture mass. Channel direction, wall thickness and support position must be reviewed together to prevent edge damage and excessive bending.

Mullite–Cordierite Extruded Batts (also known as kiln shelves or plates) are advanced ceramic refractory products used as primary support surfaces inside industrial and pottery kilns. It combines a cordierite phase (low thermal expansion), a mullite phase (high-temperature mechanical strength), and a minor glass phase, with chemical composition: typically comprises aluminum silicate, Al₂O₃ (~35%–45%), SiO₂ (~45%–55%), and MgO (≥6.5%).
Extruded Batt manufactured via vacuum extrusion, featuring internal hollow channels or ribs running through the center. Compared to solid cast batts, this design is thicker yet significantly lighter, Extruded Batts are with excellent Thermal Shock Resistance for exceptional ability to withstand rapid heating and cooling cycles without cracking; high Load-Bearing Capacity for Internal channel extrusion provides superior structural strength and warp resistance under heavy stack loads; lightweight Efficiency for offers a weight reduction of roughly 35% to 50% compared to traditional solid slabs, translating to energy savings during kiln cycles. It operates in temperature, typically rated for continuous service temperatures up to 1250°C–1350°C (though material degradation can occur past these limits).
Primary Applications
- Ceramics Industry: Firing tableware, sanitary ware, floor and wall tiles, and pottery.
- Electrical & Technical Ceramics: Supporting porcelain insulators and powder calcination processes.
- Glass and Metallurgy: Used in low- to medium-high-temperature annealing or heat-treatment furnaces.


Technical Specification
These tables describe the material or product family. Confirm the applicable grade and dimensions for this component.
Technical Data
| Category | CUA | CEN | REN | EAY | TOB | ||
|---|---|---|---|---|---|---|---|
| Chemical Composition | Al₂O₃ | % | 40 | 41 | 36 | 41 | 46 |
| SiO₂ | % | 49 | 48 | 52 | 47 | 44 | |
| MgO | % | 6.5 | 7.0 | 7.0 | 7.0 | 6.0 | |
| Bulk Density | g/cm³ | 1.95 | 1.90 | 1.85 | 1.95 | 2.00 | |
| Apparent Porosity | % | 26 | 28 | 28 | 26 | 25 | |
| M.O.R. @ 1250°C | MPa | 14 | 13 | 10 | 15 | 17 | |
| C.T.E. @ 20°C–1000°C | 10⁻⁶ K⁻¹ | 2.3 | 2.3 | 2.6 | 2.2 | 3.1 | |
| Thermal Shock Resistance | Rating | ★★★★ | ★★★★ | ★★★ | ★★★★ | ★★★ | |
| Max Working Temperature | °C | 1270 | 1250 | 1250 | 1250 | 1270 | |
Basic Dimension & Performance
| Code | Thickness | Width (mm) | Available Length (mm) | Unit Weight (kg/m) | Unit Weight (kg/m²) | Max Load @ 1200°C (kg/500 mm) |
|---|---|---|---|---|---|---|
| DDEB1 | 20 mm | 450 | 900 | 12.2 | 28.5 | 25 |
| DDEB2 | 25 mm | 440 | 900 | 13.1 | 29.8 | 38 |
| DDEB2 | 25 mm | 450 | 900 | 13.5 | 30.0 | 40 |
| DDEB2 | 25 mm | 500 | 900 | 16.4 | 32.8 | 45 |
| DDEB3 | 30 mm | 260 | 1000 | 9.1 | 35.0 | 45 |
| DDEB3 | 30 mm | 500 | 1000 | 17.5 | 35.0 | 60 |
| DDEB4 | 38 mm | 300 | 1000 | 13.7 | 45.5 | 102 |
| DDEB4 | 38 mm | 400 | 1350 | 18.5 | 46.3 | 140 |
| DDEB4 | 38 mm | 420 | 1480 | 20.0 | 47.6 | 150 |
| DDEB4 | 38 mm | 440 | 1480 | 21.0 | 47.7 | 157 |
| DDEB4 | 38 mm | 450 | 1480 | 21.4 | 47.6 | 160 |
| DDEB4 | 38 mm | 460 | 1480 | 22.2 | 48.2 | 164 |
| DDEB4 | 38 mm | 480 | 1480 | 24.2 | 50.4 | 170 |
| DDEB4 | 38 mm | 500 | 1480 | 23.3 | 46.6 | 175 |
| DDEB4 | 38 mm | 510 | 1480 | 23.5 | 46.1 | 180 |
Technical specifications
| Parameter | Selection / acceptance requirement |
|---|---|
| Material / grade | Hollow / Extruded Mullite–Cordierite Batts |
| Dimensions & tolerances | To approved drawing; catalogue size range not yet verified |
| Density / apparent porosity | Grade-specific values and test method to be confirmed |
| Strength / thermal properties | Supplier grade datasheet required before quotation |
| Temperature / load limit | Confirm for atmosphere, support arrangement and operating cycle |
| Inspection | Dimensions, visible defects and agreed batch documentation |
Selection and acceptance requirements are confirmed for the proposed grade and operating conditions. Request the supplier grade datasheet before ordering; the requirements above are not a certified technical datasheet.
Customizing service is available upon technical drawing or sketch from customers.
Technical supportApplication Photos
View 01
View 02
View 03Detail tiles are crops of the referenced photograph, not additional installations. Application and assembly references are not claimed DADATEC customer installations; confirm the material grade for your process.